PRECIPITATION-HARDENING STAINLESS STEEL

17-4PH Stainless SteelUNS S17400 · Type 630 · EN 1.4542

Kongfang Metal supplies 17-4PH stainless steel plate, sheet, bars, shapes, forgings and machined components, backed by our own stock, warehousing and processing. Also known as Type 630, UNS S17400 or EN 1.4542, this precipitation-hardening grade combines high strength with moderate corrosion resistance. Choose the delivery and aging condition for your part.

H900–H1150MPlate & sheetBarForgingsTraceable documentation on request
Polished 17-4PH stainless steel bars and rods
Specify the conditionH900, H1025, H1075, H1150 or an approved route
Match the product standardASTM or AMS route depends on the supplied form
Define acceptanceDimensions, testing, documents and delivery requirements
Available forms and supply options

Available Forms and Supply Options

Order 17-4PH as stock material, cut sizes or components prepared to your drawing. Send the form, dimensions and quantity, together with the required condition or specification. Our quotation brings the material, processing, documents and delivery details together.

Supply summary

Choose the material, processing and documentation needed for your order.

Product formsFor plate, sheet, bar, shapes, forgings or machined components, include the required form, dimensions and tolerances. Attach the drawing for a custom shape or finished component.
Condition and processingSpecify Condition A or the required aged condition, cutting dimensions, machining allowance and any heat-treatment steps. State the delivery condition and the final part condition separately.
Documents and inspectionList the required mill test certificate (MTC), heat/lot traceability, PMI, hardness, tensile or impact testing, NDT, third-party inspection and packing photographs. Include the test method, sampling and reporting requirements where specified.
Quote basisYour quotation covers the specified material, dimensions, quantity, processing, documents, price and delivery plan.
First enquiryYou may mark unknown fields as “Not specified” and send the drawing, application or target properties. Open points can be clarified before a formal quotation.
17-4PH heat-treatment conditions

17-4PH Heat-Treatment Conditions

Separate the material's delivery condition from the final condition required for the part. Condition A is the solution-treated starting condition; H900 through H1150M are distinct aging routes with different strength, hardness, ductility and impact behavior.

H900
Peak strength and hardness
ToughnessStrength
  • Typical yield strength: 1,262 MPa
  • Typical tensile strength: 1,365 MPa
  • Check impact, stress-corrosion cracking (SCC) exposure and service temperature
H1025 / H1075
High strength with more toughness
ToughnessStrength
  • Useful middle range for many high-strength parts
  • Use the table below to compare H1025 and H1075
  • Define minimum properties, impact and test direction
H1150
Higher ductility and impact energy
ToughnessStrength
  • Single aging step after solution treatment
  • Lower typical strength than H900–H1075
  • Confirm impact and service requirements
H1150M
Distinct two-step overaging route
ToughnessStrength
  • Not interchangeable with H1150
  • Lower typical strength and hardness than H1150
  • Confirm the complete approved heat-treatment sequence
Ordering boundary: do not write only “17-4PH” or assume Condition A is suitable for service. State the condition to be delivered, who performs any later aging treatment, and the final properties or hardness that control acceptance.
Specifications and grade designations

Specifications and Grade Designations

A designation identifies the alloy family. It does not replace the product-form standard, delivery condition, dimensions, testing or customer specification.

Common designations

UNSS17400
Type630
EN1.4542
EN nameX5CrNiCuNb16-4
JISSUS 630
Common name17-4PH

Use the grade equivalent chart to identify candidates, then verify the governing product standard.

ASTM A564Bars and shapes: state form, size, condition, tolerance and tests.
ASTM A693Plate, sheet and strip: state dimensions, finish, condition and flatness requirements.
ASTM A705Forgings: define geometry, condition, test direction/location and inspection scope.
AMS 5604Aerospace sheet, strip and plate: confirm revision and approval requirements.
AMS 5622 / 5643Bar and forging routes: use the drawing or customer specification; do not assume interchangeability.
Material data

Chemical Composition and Typical Physical Properties

Use these published values for identification and preliminary calculations. The governing purchase specification and certified test results control acceptance.

Chemical composition

Common Type 630 / UNS S17400 limits, weight percent.

ElementLimit, wt.%
Chromium15.00–17.50
Nickel3.00–5.00
Copper3.00–5.00
Niobium + tantalum0.15–0.45
Carbon0.070 max.
Manganese1.00 max.
Silicon1.00 max.
Phosphorus0.040 max.
Sulfur0.030 max.
IronBalance

Physical-property snapshot

Condition matters; avoid treating one catalogue value as a certified lot result.

Density7,750 kg/m³Condition A; Carpenter reports 7,800–7,820 kg/m³ for H900–H1150.
Magnetic responseGenerally magneticThe martensitic structure produces a magnetic response. A magnet test does not verify grade or condition.
Alloy structureMartensitic PH stainlessHigh strength develops through controlled solution treatment and aging.
Main aging responseCopper precipitationThe selected aging condition changes strength, hardness, ductility and impact behavior.

Composition and density: Carpenter Custom 630 datasheet. Magnetic response is consistent with Carpenter's description of martensitic stainless steels; use PMI, chemistry and the purchase standard for material verification.

Typical room-temperature mechanical properties by condition

Compare the typical properties for each aging condition below. Set the required acceptance values in the purchase specification.

ConditionAging treatment after solution treatmentTypical yieldTypical tensileTypical hardness
H900482°C / 900°F, 1 h, air cool1,262 MPa1,365 MPa44 HRC
H1025552°C / 1025°F, 4 h, air cool1,117 MPa1,158 MPa38 HRC
H1075580°C / 1075°F, 4 h, air cool1,020 MPa1,131 MPa36 HRC
H1150621°C / 1150°F, 4 h, air cool869 MPa993 MPa33 HRC
H1150M760°C / 1400°F for 2 h, air cool; then 621°C / 1150°F for 4 h, air cool600 MPa848 MPa29 HRC

Typical room-temperature values from Carpenter Technology's Custom 630 datasheet—not guaranteed minimums for every order. H1150 and H1150M are separate heat-treatment routes. Product form, section size, melt route and test details can change results, so the purchase specification and certified test results govern acceptance.

Corrosion resistance and service limits

Corrosion Resistance and Service Limits

The grade works best when high strength and moderate stainless corrosion resistance are needed together. It is not a universal chloride upgrade.

Start with 17-4PH when…

  • The part needs substantially higher strength or hardness than annealed 304/316.
  • The actual environment is compatible with moderate stainless corrosion resistance.
  • The drawing and supply chain can control the final aging condition.
  • Lot traceability and final-condition verification can be defined.

Compare another alloy when…

  • Continuous seawater, warm chlorides, crevices or strong reducing acids dominate.
  • The fabrication route needs extensive cold forming.
  • Low-temperature impact requirements are critical but not defined by condition and test.
  • The design temperature conflicts with the aging condition.
Stainless steel components exposed to moisture

Do not choose from the word “stainless” alone

Define chloride level, temperature, pressure, cleaning chemicals, crevices, deposits and whether exposure is continuous or intermittent. Carpenter rates seawater resistance as restricted.

Typical applications

Typical Applications and Buyer Checks

Match the part geometry, service environment, final heat-treatment condition and acceptance tests to the application.

Pump shafts and valve stems

Check first: chloride level, continuous or intermittent exposure, required condition, straightness and NDT.

Fasteners, gears and precision parts

Check first: H900 versus H1025/H1150, thread or finished geometry after heat treatment, hardness and impact requirements.

Process and energy components

Check first: pressure or customer code, corrosion medium, test direction, traceability and any third-party inspection.

Aerospace or drawing-controlled work

Check first: exact AMS revision, melt route, approved source, lot testing and deviation control. A matching grade name is not enough.

If the drawing calls for a different PH grade, compare the required specification and condition before substituting. See 15-5PH stainless steel for the neighboring grade family.
Fabrication and heat-treatment planning

Fabrication and Heat-Treatment Planning

Machining, forming, welding and heat treatment can change dimensional control, toughness, corrosion performance and the final acceptance route.

Machining

Agree when the part will be aged

State the stock condition, machining stage, heat-treatment allowance, final hardness, straightness and any nondestructive testing.

Forming

Cold formability is limited

Confirm bend radius, rolling direction, intermediate processing and final heat treatment before ordering material for significant forming.

Welding

Filler and post-weld treatment are linked

E/ER630 is a common matching filler starting point. Post-weld treatment depends on the material condition before welding and the qualified welding procedure.

T°

High-temperature service

ASTM A564 and A693 describe high-strength use generally up to about 315°C / 600°F. A higher short-term oxidation limit is not an approved continuous design temperature.

−°

Low-temperature impact requirements

Impact performance depends strongly on condition. State test temperature, specimen orientation, minimum impact energy and acceptance standard for critical parts.

Order documentation and inspection

Order Documentation and Inspection

Send the dimensions, quantity and application you already know. Our team will help you complete the material and processing requirements for a quotation.

Define the part

Product form, approximate size, quantity, drawing and end use.

Confirm the specification

Grade, governing standard, revision and required aging condition.

Agree acceptance

Tolerance, mechanical tests, impact, PMI, NDT, inspection and documents.

Confirm delivery

Destination, required date, packaging, marking and Incoterm.

Mill test certificateHeat / lot traceabilityHardness or tensile testImpact test where specifiedPMI / NDT where specifiedThird-party inspectionMarking and packaging

Include the required documents, tests and inspection stages in your RFQ so they can be priced and scheduled.

Supply, inspection and documentation examples

Supply, Inspection and Documentation Examples

Browse the 17-4PH ingot certificate and examples of on-site inspection, packaging and container loading.

17-4PH ingot inspection certificate showing heat FG26P311 and chemical composition

Redacted supplier inspection certificate

The redacted supplier certificate identifies a 17-4PH ingot, heat FG26P311, and records chemical composition.

Handheld instrument in contact with metal material during an on-site inspection

On-site inspection activity

On-site inspection with a handheld instrument.

Kongfang Metal wooden crate marked 155 by 20 by 2000 millimetres

Packaging and size identification

The crate label shows Kongfang Metal packaging and a 155 × 20 × 2000 mm size reference.

Forklift loading strapped metal packages into a shipping container

Shipment handling

Strapped metal packages are shown during container loading.

For an order-specific evidence package: state the required material marking, certificate type, testing, traceability and packing records before quotation.
Request a 17-4PH quote

Request a 17-4PH Quote

For the first conversation, send the product form, approximate dimensions, quantity, application and target condition you already know. Unknown fields can remain “Not specified” until the technical route is clarified.

RFQ example
“17-4PH round bar, about 40 mm diameter, approximately 2 tonnes, for pump shafts exposed to intermittent chloride washdown. Please compare H1025 and H1150. MTC and heat/lot traceability required. Delivery to Hamburg; please state earliest lead time.”
Quotation checklist

Information for a formal quotation

Grade17-4PH / Type 630 / S17400
Product formPlate, bar, forging or component
StandardASTM, AMS, EN or customer spec
Delivery conditionCondition A, H900, H1025, H1075, H1150…
Final part conditionSame as supplied, or aging route and acceptance properties
DimensionsSize, length, tolerance and machining allowance
QuantityPieces and total weight
TestingMTC, PMI, impact, NDT or TPI
DeliveryDestination, required date and Incoterm
AttachmentsDrawing, customer specification or reference photo

For aerospace, pressure-equipment, sour-service or customer-approved work, send the complete drawing, specification revision, approved-source requirements and acceptance tests with your RFQ.

Frequently asked questions

17-4PH Ordering Questions

Is 17-4PH the same as Type 630?

Type 630 and UNS S17400 identify the alloy family commonly called 17-4PH. EN 1.4542 and SUS 630 are corresponding designations, but product standards and delivery conditions are not automatically interchangeable.

Is H900 always the best condition?

No. H900 is a starting point for maximum strength and hardness. H1025, H1075 and H1150 provide different toughness, ductility and stress-corrosion balances. Select against the full mechanical and environmental requirement.

Can 17-4PH be used in seawater?

Do not approve it from the grade name alone. Supplier data rate seawater resistance as restricted. Continuous immersion, temperature, crevices, deposits, flow and stress can change the result; compare 316L, duplex or another alloy when chloride resistance dominates.

Is 17-4PH magnetic?

Yes, it is generally magnetic because it has a martensitic structure. A simple magnet response cannot identify the grade, confirm its heat-treatment condition or qualify it for a magnetic-performance requirement; use the specified material tests instead.

What density should be used for 17-4PH weight calculations?

Carpenter publishes 7,750 kg/m³ (0.2800 lb/in³) for Condition A and 7,800–7,820 kg/m³ for H900 through H1150. Use the value for the specified condition when the difference matters, and use certified dimensions and actual mass for commercial acceptance.

Can 17-4PH be welded and then aged?

Post-weld treatment depends on the material’s condition before welding. Material welded in Condition A may be aged directly when the specified properties can be met. Material welded in an overaged condition requires solution treatment before final aging. Confirm the sequence through the qualified welding procedure.

en_USEN
Send Your Inquiry Today

Scan to add on WeChat

Kongfang Metal WeChat-QR-Code