FERRITIC STAINLESS STEEL

409 Stainless Steel Supplier

409 is a magnetic ferritic stainless steel used extensively in automotive exhaust systems.

Kongfang Metal supplies 409 sheet, coil, strip, tube and processed stainless steel products.

Exhaust tubing and formed metal components

It combines a relatively low alloy content with useful resistance to oxidation and corrosion, making it a practical choice for formed and welded components where a bright decorative finish is not the main requirement.

We use our warehousing and processing facilities to prepare slit strip, cut sheets and blanks for your production requirements, with material documentation and export packaging.

Start with the product form, dimensions or drawing, quantity and intended use. If your specification is still being finalised, send the details you have and tell us what the part will be used for.

Available Forms and Processing

Our slitting, cut-to-length and cutting services prepare material for your production line.

Sheet, Coil and Strip Supply

Dimensions below are in millimetres. Sheet and plate sizes are thickness × width × length.

ProductAvailable sizesSurface and delivery conditionSupply method
Cold-rolled coilThickness 0.4–3.0; widths 1,000 / 1,219 / 1,250 / 1,5002B or 2D; annealed and pickled; in coilStock thicknesses include 0.8 / 1.0 / 1.2 / 1.5 / 2.0; special sizes to order
Cold-rolled sheet0.4–3.0 × 1,000–1,500 × 2,000–3,0002B or 2D; cut-to-length or standard sheetsStock sheets and sheets cut from coil
Hot-rolled coilThickness 3.0–6.0; width 1,000–1,500No.1; hot rolled, annealed and pickledStock material
Hot-rolled plate3.0–12.0 × 1,000–1,500 × 2,000–6,000No.1; annealed and pickled; cut to sizeStock thicknesses 3.0–6.0; thicker material quoted to order
Slit stripThickness 0.3–2.0; width 10–6002B or 2D; slit edges; in coilSlit to width; special tolerances to order

Welded Tube Supply

ProductAvailable sizes in mmSurface and conditionSupply method
Welded round tubeOutside diameter 19.1–101.6; wall 1.0–2.0; usual length 6,000Mill finish; as-welded or with specified post-weld treatmentSelected common exhaust-tube sizes in stock; other sizes to order
Made-to-order welded tubeOutside diameter 102–153; wall 1.2–5.0Mill finish or pickled; weld treatment to specificationProduction to order for the specified size, grade and manufacturing requirements

Your quotation confirms the size combination, stock quantity, processing and dispatch schedule for the order.

Project Products

Seamless tube and round bar are quoted against the project specification. The sizes below are reference ranges for a project enquiry; the quotation identifies the manufacturing method, delivery condition and required tests.

ProductReference sizes in mmDelivery and processing options
Seamless tubeOutside diameter 16–114; wall 1.5–8.0Heat-treatment condition and surface finish to the specified product standard and order.
Round barDiameter 10–100; length 1,000–6,000Hot-rolled supply; heat treatment to specification; peeled or machined surface to order.

Stock, Processing and Trial Orders

Shearing, laser cutting and bending can be included to produce parts from your drawing.

For a trial batch, send the first-run quantity and the expected repeat quantity. We can compare a cut or slit order with a full-coil or production order. The quotation will state the minimum order quantity, processing, documentation and lead time for that supply option.

For BA, No.4 or hairline (HL) finishes, include the required appearance or a sample with the enquiry so the finish and starting material can be agreed together.

Coil and Slit Strip

Coil and slit strip feed tube mills, roll-forming lines and presses. The required width, coil inside diameter and maximum coil weight should match your uncoiling equipment; edge quality matters where the strip will be welded or expanded.

For tube-making strip, specify the strip width and the required finished tube wall thickness. For expanded tube ends, include the expansion requirement and any specified seam tests.

View stainless steel coil

Sheet, Plate and Cut Blanks

For cut blanks, the drawing should show the finished size and any forming or machining allowance.

For a visible panel, tell us which face will be exposed and send a surface sample or finish requirement. For a pressed part, send the drawing and identify the critical bends, holes and formed areas.

View plate and sheet options

Tube Requirements

For welded exhaust tubing, the seam and any bend or expansion requirements are important parts of the specification. Project enquiries for other tube products should include the product standard and manufacturing method as well as the outside diameter, wall thickness and length.

409 Grades and Standards

409 is a family of stabilised ferritic grades. [4] For ASTM flat-product orders, the purchase description combines ASTM A240/A240M with the specified UNS designation. For tubing, agree the product specification, grade and delivery condition together, and match them to the supplied material certificate. The product standard and its edition determine the applicable composition, condition and tests.

DesignationHow to use it on an enquiry
Type 409State the product specification and full grade designation alongside the common name
UNS S40910, S40920 or S40930Identify the particular variant required by the drawing or material specification
UNS S40900A designation found in older 409 references; retain the exact specification when replacing an existing component
EN 1.4512 / X2CrTi12The European titanium-stabilised ferritic grade commonly associated with 409
SUS or GB designationCopy the complete designation and product standard from the project requirement

Your quotation will identify the proposed grade and product specification, together with the material documentation. If substitutions are permitted, confirm the chemistry, required tests and documentation before placing the order. For dual-certified material, both designations and the applicable results should appear on the mill test certificate (MTC).

Chemical Composition

EN 1.4512 Flat Products to EN 10088-2

ElementMass percent
Carbon, C0.030 maximum
Chromium, Cr10.5–12.5
Silicon, Si1.00 maximum
Manganese, Mn1.00 maximum
Phosphorus, P0.040 maximum
Sulfur, S0.015 maximum
Titanium, Ti6 × (C + N) minimum; 0.65 maximum

EN 1.4512 / X2CrTi12, EN 10088-2:2024 composition. C and N in the titanium formula are the carbon and nitrogen mass percentages. [1]

For an ASTM order, use the chemistry requirements for the specified UNS variant and product standard. The EN 1.4512 table provides the European flat-product reference.

Mechanical Properties

EN 1.4512 Annealed Flat Products at Room Temperature

ProductMaximum thickness in this table0.2% proof strength minimumTensile strengthElongation minimum
Cold-rolled strip8 mm210 MPa longitudinal; 220 MPa transverse380–560 MPa25%
Hot-rolled strip13.5 mm210 MPa longitudinal; 220 MPa transverse380–560 MPa25%

EN 10088-2:2024, annealed condition. For thickness below 3 mm, the published elongation provisions use an 80 mm gauge length, with a permitted 50 mm alternative specimen; for thicker material, a proportional gauge length applies. [2]

Longitudinal means along the rolling direction; transverse means across it. When comparing certificates, check whether proof strength was measured longitudinally or transversely. The thickness column defines the scope of this property table. Supply options are listed above; finished tubes and components follow their own specified tests.

Corrosion, Surface Rust and Exhaust Service

409 is widely used where functional performance matters more than a permanently bright surface. It has lower general corrosion resistance than higher-chromium ferritic grades such as 430 and austenitic grades such as 304. Brown surface staining can develop in service, particularly with road salt, retained moisture or corrosive condensate.

For an exhaust part, consider the two sides of the wall separately. The inside sees exhaust gas and condensate; the outside may see water, road salt and dirt trapped around joints or brackets. Drainage and the amount of time the part stays wet can change the selection.

For replacement work, tell us where the part failed. A perforated low point, a cracked weld and surface staining on an otherwise sound panel call for different checks. Photographs of the failure area, together with wall thickness and operating conditions, help identify the material and fabrication requirements.

Heat and Thermal Cycling

An exhaust assembly sees changing temperatures, restraint and vibration. Ferritic steels generally expand less than austenitic grades, which is useful in thermally cycled assemblies. The weld design and attachment points still need to accommodate movement.

The useful starting point is the component metal temperature, including sustained duty and short peaks. A manifold near the engine, a downstream muffler that stays wet after short trips, and a restrained welded bracket present different problems. Assess hot-end parts for oxidation and thermal fatigue, wet downstream sections for condensate attack, and attachments for movement and vibration. An oxidation-temperature figure alone does not establish an exhaust-system rating.

Forming and Welding

Press-brake forming of stainless steel sheet

Forming Coil and Sheet

For roll forming, pressing or tube expansion, specify the final shape and the areas with the greatest deformation. Bend radius, edge quality, thickness variation and tool condition can all affect the result.

For a pressed or expanded part, a drawing that marks the critical bend or expansion area is more useful than a description such as “good formability”. It gives the material, tooling and welding teams a specific feature to assess.

TIG welding of stainless steel tube

Welding 409

409 is commonly welded in thin-section exhaust fabrication. Ferritic stainless steels need control of welding heat input because grain growth can reduce joint toughness. Joint thickness, restraint and the required service performance influence the procedure.

Use a qualified welding procedure specification (WPS) to select the filler, heat input, shielding and sequence. Matching ferritic and suitable austenitic fillers are used for different joints; a generic filler list is not a substitute for selecting one for the actual assembly. [3]

Mechanical surface finishing of stainless steel

Cleaning After Fabrication

Remove fabrication contamination and weld residues using a cleaning method suited to the product and its finish. Keep carbon-steel grinding debris and tooling contamination away from the stainless surface. Where appearance matters, agree on a reference sample and the required finish before production.

409 vs 430, 410 and 304

MaterialWhen to consider itWhat to compare
409Formed and welded exhaust or heat-related components with cost-sensitive requirementsCondensate, salt exposure, forming demands and weld performance
430Ferritic products needing more corrosion resistance and a controlled visible finishFormability, welded details and the required appearance
410Parts selected for hardening and mechanical propertiesHeat-treated condition, toughness and welding requirements
304Parts needing better corrosion resistance than 409 or a cleaner visible surfaceCondensate and salt exposure, surface finish, greater thermal expansion and the completed assembly cost

For a concealed exhaust component, some surface staining may be acceptable if the required wall life and joint performance are achieved. For a visible tailpipe or exposed cover, appearance can justify comparing 304 and the specified finish. Persistent salty moisture or aggressive condensate needs a closer corrosion assessment; choosing 304 by name alone does not resolve every exposure.

Compare the cost of slit or cut material, forming scrap, tooling, welding, finishing and replacement, as well as the base metal. A lower sheet price may not reduce the finished part cost if forming causes more scrap or rework, or the material does not provide the required service life.

Explore 430 stainless steel, 410 stainless steel and 304 stainless steel for a closer comparison.

Applications

409 is established in exhaust tubing, muffler bodies and related formed components. It is also used in selected heat-exchanger, heater and ducting applications where the service conditions suit the grade.

For new designs, assess the grade in the finished assembly, particularly where the part carries pressure or handles corrosive condensate.

Packing and Dispatch at Kongfang Metal

We retain heat identification during size preparation and pack material for handling and transport. Surface protection and package sizes are agreed with the order.

Protective wrapping of stainless steel material at Kongfang Metal
Protective wrapping of stainless steel material at Kongfang Metal
Forklift handling during container loading at Kongfang Metal
Forklift handling during container loading at Kongfang Metal

Explore our processing services.

Documentation and Receiving Checks

The MTC, material marking and package labels should identify the same heat and grade. Before releasing material to production, check the product specification, dimensions, finish and reported properties.

For slit strip, also check width, edge condition and coil identification. For tube, check the ordered wall, ends and any specified weld or dimensional test records. Review the records for inspection or sample approval required before shipment.

Keep the heat identification with the material after cutting. A magnetic response confirms neither the grade nor the stabilisation requirements, because several stainless steel families are magnetic.

Frequently Asked Questions

Does 409 stainless steel rust?

Yes. Surface staining or rust can occur, especially with salt, retained moisture and condensate. For a functional exhaust component, assess wall loss and the condition of welds as well as appearance. For a visible decorative part, compare a more corrosion-resistant grade and the required finish.

Is 409 magnetic?

Yes. Its ferritic structure makes it magnetic. Magnetism alone cannot distinguish 409 from other magnetic stainless steels.

Can 409 be welded?

Yes. It is widely welded in thin exhaust components. Use a procedure that controls heat input and selects a filler suited to the joint and service conditions.

Is 409 cheaper than 304?

409 usually has a lower alloy cost because it relies much less on nickel. Compare quotations for the same dimensions, product condition, processing and inspection scope to assess the cost of the finished part.

Is 409 the same as 409L?

409L is used as a low-carbon designation in some product and market descriptions. The complete grade designation and product specification identify the chemistry and tests required by the order. Our 409L stainless steel page covers that related material; use the drawing and certificate to compare a particular supply.

What is the difference between 409 and 1.4512?

409 is a common type designation; 1.4512 is the European steel number for X2CrTi12. The exact requirements come from the specified product standard. The EN composition and flat-product properties shown above belong to 1.4512.

Request a 409 Quote

Start an Enquiry

Send the product form, any dimensions or drawing, quantity and intended use. You can contact us while the specification is still being finalised. For a replacement exhaust part, a photograph of the part and its position in the system is a useful starting point.

Details for a Formal Quotation

  • Material: complete grade designation, product standard and edition, delivery condition and finish.
  • Sizes and processing: dimensions, tolerances, quantity, slit-edge or coil requirements, and cutting or fabrication work.
  • Inspection and delivery: MTC, agreed tests, packaging, destination and required delivery date.

For exhaust or heat-related parts, add the part location and operating conditions. Your quotation will state the material, processing, documents, minimum order quantity and lead time.

en_USEN
Send Your Inquiry Today

Scan to add on WeChat

Kongfang Metal WeChat-QR-Code