MARTENSITIC STAINLESS STEEL

SUS420J2 Stainless SteelJIS SUS420J2 · EN 1.4028 / X30Cr13

Kongfang Metal supplies SUS420J2 stainless steel sheet, coil, strip, bar and cut blanks, with our own stock, warehousing and processing services. This hardenable martensitic grade is used for cutting and wear components. Tell us the required form, dimensions and final hardness, or send the part drawing.

Cutlery & bladesWear componentsSheet, strip & blanksFinal hardness must be agreed
SUS420J2 stainless steel sheet and machined parts
Confirm the designationSUS420J2 commonly cross-references to EN 1.4028, not 1.4034
Separate supply from final conditionAnnealed material is commonly processed before hardening
Define acceptanceHardness, test method, dimensions and traceability
Quick selection guide

Start With the Requirement, Then Confirm the Grade

SUS420J2 is useful when hardness and wear resistance matter, but it is not the default answer for every 420-family drawing, chloride environment or welded assembly.

If your drawing or application needsStart withCheck before ordering
A JIS cutlery or wear grade with more hardening potential than SUS420J1SUS420J2Product standard, annealed delivery condition, final heat-treatment route and hardness acceptance method
An EN-designated grade close to SUS420J2EN 1.4028 / X30Cr13Confirm the product standard and full chemistry; a cross-reference is not blanket approval for substitution
A higher-carbon EN blade gradeEN 1.4034 / X46Cr13Do not relabel it as SUS420J2; compare chemistry, hardness, toughness and the drawing requirement
High resistance to salt or persistent chloride exposureReconsider the grade420-family martensitic grades are not the default choice for demanding chloride service
A welded assemblyReconsider the joint or gradeSUS420J2 is difficult to weld; use a qualified welding and heat-treatment procedure if welding is unavoidable
Core purchasing rule: if a drawing says “420J2 / 1.4034,” stop and resolve the designation before issuing the purchase order.
Available forms and supply options

SUS420J2 Stock and Processing

We supply SUS420J2 sheet, coil, strip, bar and cut blanks, with processing to your specified dimensions or drawing.

Supply summary

Prepare your quotation request with the material, processing, document and delivery requirements below.

Flat-product processingFor flat products, we provide slitting and cut-to-length processing. Send the thickness, finished width or length, and any edge or tolerance requirements.
Bars and blanksFor bar or cut blanks, include the section size, cut length, tolerances and machining allowance shown on the drawing.
Documents and inspectionMill test certification, heat or lot traceability, hardness testing, chemical verification and third-party inspection can be requested.
Quote basisYour quotation sets out the material specification, processing, documents, inspection, price and delivery plan.
First enquiryIf the delivery condition is unknown, send the application and target hardness. Open points can be clarified before the formal quotation.
Grade identity

SUS420J2, EN 1.4028 and EN 1.4034

“420” does not describe one universal chemistry. Carbon content and the governing product standard change hardening response, toughness and corrosion behaviour.

DesignationHow to use it in a purchase specificationCarbon referencePractical meaning
JIS SUS420J1A lower-carbon JIS martensitic grade0.16–0.25% in published JIS-grade screening dataLower quench hardness than SUS420J2; often considered where ductility or formability carries more weight
JIS SUS420J2The primary grade covered by this page0.26–0.40% in published SUS420J2 screening dataHigher quench hardness than SUS420J1; associated with cutlery and wear parts
EN 1.4028 / X30Cr13A commonly used EN cross-reference for SUS420J20.26–0.35% in published EN-grade screening dataSuitable for comparison, but the governing product standard and required properties still need confirmation
EN 1.4034 / X46Cr13A separate higher-carbon 420-family gradeApproximately 0.45% in published EN-grade screening dataHigher hardening potential; not an automatic substitute for SUS420J2 or 1.4028
When several designations appear on one drawing: ask which standard controls acceptance. Do not carry an unresolved mismatch into the purchase order.
Published material data

Composition, Annealed Supply and Hardening Response

The following published data support grade comparison. Specify the product standard and delivery condition, then use the supplied heat’s test results for acceptance.

Chemical composition

Published SUS420J2 screening values, mass %.

ElementPublished value
Carbon (C)0.26–0.40
Silicon (Si)≤1.00
Manganese (Mn)≤1.00
Phosphorus (P)≤0.040
Sulfur (S)≤0.030 in the published screening data
Chromium (Cr)12.00–14.00

The order must specify the governing product standard and any agreed additional chemical limits.

Annealed delivery condition

Published values for an annealed SUS420J2 flat-product condition.

PropertyPublished value
0.2% proof stress≥225 MPa
Tensile strength≥540 MPa
Elongation≥18%
Hardness≤99 HRB / ≤247 HV

These published values refer to annealed flat products. Specify the product standard, thickness and delivery condition for the order, together with the test direction where required.

Published hardening examples

Useful for setting the discussion

A published SUS420J2 screening example reports approximately HV630 / HRC57 after quenching, while published EN 1.4028 screening data show 45–51 HRC under a stated final heat-treatment basis. These figures describe different source products and must not be combined into one acceptance value.

Not a blanket order promise

Final properties depend on the complete route

Compare the chemistry, starting condition, section size and complete quench-and-temper cycle alongside each published hardness value. Set the required final condition and hardness on the order.

Include in the RFQ, as applicable: the required delivery condition; target hardness range and test method; and the governing drawing or qualified heat-treatment procedure. For heat-treated material, agree the required properties and test methods before ordering.
Corrosion resistance and application fit

Service Limits and Selection Checks

SUS420J2 provides moderate corrosion resistance. Use it where hardness and wear are central and the environment is controlled; reassess the alloy when chloride exposure or welding drives the design.

Reasonable starting point

Hardness and wear dominate

A hardened, smooth or polished surface generally gives better corrosion performance than a rough surface or unsuitable heat-treatment condition. Cleaning, drying and surface condition remain important.

Cutlery blanksCutting partsMeasuring toolsValve and wear components
Separate material assessment

Persistent chloride or seawater exposure

Temperature, crevices, chloride cleaners, acidic residues and long wet holding periods can change the result. Compare another alloy when corrosion resistance dominates.

SeawaterSalt exposureChloride cleanersWelded assemblies
Applications and key selection checks

Connect the application to a measurable requirement

Select the material and heat treatment for the cutting, wear or dimensional requirements below.

  • Knife or cutting blank: final hardness, edge geometry, toughness, corrosion exposure and distortion allowance.
  • Valve seat or wear component: contact stress, wear mechanism, corrosion medium, finish and dimensional stability after heat treatment.
  • Measuring tool or straightedge: hardness, flatness, dimensional stability, finish and calibration environment.
  • Food-contact article: intended food, contact time and temperature, cleaning chemicals, market-specific compliance and finished-surface condition.

Use in cutlery does not by itself certify a finished article for food contact. Grade selection is only one part of the finished-article assessment.

Fabrication and welding

Plan Processing Around the Final Condition

Complete blanking and most machining while the material is annealed, then control distortion, finishing and verification through the agreed heat-treatment route.

01

Cutting, machining and forming

Allow for distortion and finishing after heat treatment when tolerance is tight. Cold forming is more limited than with austenitic stainless steels; check bend radius and forming sequence on the actual thickness and condition.

02

Heat treatment

Use the source mill’s data, governing standard and a qualified procedure. Record the complete cycle and test the agreed property on the finished lot when it controls acceptance.

03

Welding

Welding is not the normal first choice. If unavoidable, qualify the joint, filler, preheat, interpass control, cooling and post-weld treatment together; do not select a filler from a generic grade-page recommendation.

Receiving inspection

Six Checks Before Material Enters Production

Receiving inspection should protect grade identity, traceability and the properties that the drawing or purchase order actually requires.

1

Match the documents

Purchase order, packing list and certificate should use the same grade, standard, product form and condition.

2

Protect traceability

Heat or lot identification should match the certificate and remain identifiable after cutting.

3

Inspect dimensions and surface

Check tolerances, edge condition, straightness or flatness, and the agreed surface finish.

4

Read the actual results

Verify required chemistry, mechanical or hardness results. Blank fields are not test results.

5

Complete additional tests

Perform buyer-specified PMI, hardness, third-party or laboratory tests at the agreed stage.

6

Keep heats and conditions separate

Packaging should protect finished surfaces and preserve lot identification.

Carbon cannot be confirmed by handheld XRF. When carbon is needed to distinguish SUS420J1 from SUS420J2, agree a suitable method such as calibrated spark optical emission spectrometry (OES) or laboratory analysis, including sampling and acceptance requirements.
Mismatch stop: if the certificate says 1.4034 while the purchase order says SUS420J2, stop release and resolve the designation before machining or heat treatment.
Request a SUS420J2 quote

Start With What You Know

Start with the dimensions, quantity, application or drawing you have. We will help you complete the delivery-condition and processing details for a quotation.

Open the SUS420J2 enquiry form →

Initial enquiry checklist

Product formSheet, coil, strip, bar or blank
Dimensions & quantityApproximate values are enough to begin
Condition or hardnessState the target if known
Application & environmentInclude corrosion, wear and contact conditions
Drawing or standardAttach what is available
Destination & dateNeeded for sourcing and lead-time confirmation

The formal quotation should state the agreed grade and standard, product form, condition, dimensions and tolerances, processing, inspection and documentation, packaging, price and lead time.

Frequently asked questions

SUS420J2 FAQ

Is SUS420J2 the same as EN 1.4034?

No. Published grade cross-reference tables commonly align SUS420J2 with EN 1.4028 / X30Cr13. EN 1.4034 / X46Cr13 is a separate higher-carbon grade. Any substitution must be approved against the drawing, product standard and required properties.

What hardness can SUS420J2 reach?

There is no single value for every product and heat-treatment route. A published screening example reports HV630 / HRC57 after quenching, while other source products and final tempering requirements produce different ranges. Specify the target, test method and condition in the order.

Is SUS420J2 magnetic?

Yes. It is a ferromagnetic martensitic stainless steel.

Is SUS420J2 corrosion resistant?

It provides moderate corrosion resistance, and a hardened, smooth surface generally performs better than a rough or unsuitable condition. It is not the default choice for persistent chloride or seawater exposure.

Can SUS420J2 be welded?

It is difficult to weld and is not a routine welded-fabrication grade. If welding is unavoidable, use a qualified procedure covering the joint, filler, preheat, interpass temperature, cooling and post-weld treatment.

Is SUS420J2 suitable for food-contact tools?

It is used for cutlery, but the grade name alone does not establish finished-article compliance. Assess the final surface, manufacturing route, intended food and cleaning conditions, destination market and required documentation.

en_USEN
Send Your Inquiry Today

Scan to add on WeChat

Kongfang Metal WeChat-QR-Code