Alloy 255 Duplex Stainless Steel (UNS S32550 / 1.4507) Supplier

Available Forms

As a Alloy 255 stainless steel manufacturer in China, Kongfang Metal provide a wide range of Alloy 255 materials.

Cold Rolled Stainless Steel Sheet

Alloy 255 Sheet

Cold Rolled
Width: 1000 - 2000mm
Thickness: 0.3 - 6.0mm

Hot Rolled Stainless Steel Plate

Alloy 255 Plate

Hot Rolled
Width: 1000 - 2000mm
Thickness: 3 - 100mm

Cold-Rolled Stainless Steel Coil

Alloy 255 Cold-Rolled Coil

Cold Rolled
Width: 1000 - 2000mm
Thickness: 0.3 - 6.0mm

Hot-Rolled Stainless Steel Coil

Alloy 255 Hot-Rolled Coil

Hot Rolled
Width: 1000 - 2000mm
Thickness: 3 - 14mm

Stainless Steel Strip

Alloy 255 Strip

Width: 7 - 600mm
Thickness: 0.3 - 10mm

Stainless Steel Seamless Pipe

Alloy 255 Seamless Pipe

OD: ≤610mm
WT: 1 - 100 mm

Stainless Steel Welded Pipe

Alloy 255 Welded Pipe

OD: 6 - 3000mm
WT: 1 - 100 mm

Stainless Steel Round Bar

Alloy 255 Round Bar

Diameter: 1 - 200mm
Length: 100 - 12000mm

Stainless Steel Flat Bar

Alloy 255 Flat Bar

Width: 20 - 800 mm
Thickness: 3 - 60 mm

Stainless Steel Angle Bar

Alloy 255 Angle Bar

Side Length: 20 - 250 mm
Thickness: 3 - 35 mm

Stainless Steel Channel

Alloy 255 Channel

Height: 50 - 400 mm
Thickness: 4 - 20 mm

Stainless Steel H Beam

Alloy 255 H Beam

Height: 100 - 1000 mm
Thickness: 6 - 40 mm

If your project requires much higher strength than 316L and far better corrosion resistance than standard duplex grades, Alloy 255 delivers. It offers exceptional performance in seawater, brine, acids, and chloride-rich systems, while providing twice the strength of austenitic stainless steels.

Close-up of machined stainless-steel flanges and shafts representing Alloy 255 duplex stainless steel.

Standards and Equivalent Grades

Grade UNS EN DIN ISO GB
Alloy 255
S32550
1.4507
X2CrNiMoCuN25-6-3
15156-3 applicable
00Cr25Ni7Mo4N

Chemical Composition (% by weight)

Grade Standard Cr Ni Mo Cu N Mn Si C Fe
Alloy 255 / S32550
ASTM A240
24–27
5.5–7.5
3–4
1.5–2.5
0.15–0.32
≤1.5
≤1.0
≤0.03
Balance

Mechanical Properties

Property Metric Imperial
Tensile Strength
≥690 MPa
≥100 ksi
Yield Strength
≥450 MPa
≥65 ksi
Elongation
≥25%
≥25%
Hardness
≤290 HBW
≤290 HBW
Close-up photograph of two machined stainless-steel shafts with flanges, representing the high strength, corrosion resistance, and durability features of Alloy 255 duplex stainless steel.

Key Features

  • Super-duplex grade with very high strength

  • Superior chloride pitting & crevice corrosion resistance

  • Excellent resistance to stress corrosion cracking (SCC)

  • Outstanding seawater performance

  • Strong resistance to sulfuric acid and mixed acid environments

  • Good weldability compared to other super-duplex grades

  • Much more cost-effective than nickel alloys & super austenitics

Corrosion & Heat Resistance

AlloyPRENChloride Resistance
316L~25Moderate
2205~34High
255≥40Superior
250742–45Higher but similar class
Close-up photograph of two large cylindrical stainless-steel flanges with water droplets, illustrating the corrosion resistance of Alloy 255 duplex stainless steel.

Processing & Fabrication

Stainless Steel Machinability
Machining
  • Similar difficulty to 2507

  • Use rigid setups & high lubrication

Stainless Steel Weldability
Welding
  • GTAW, GMAW, SMAW, FCAW suitable

  • Use super-duplex fillers (e.g., ER2594, ER2209)

  • Avoid heat input extremes to maintain phase balance

  • Post-weld cleaning + pickling recommended

Stainless Steel Heat Treatment
Heat Resistance
  • Continuous service: up to 300–315°C (575–600°F)

  • Avoid long exposure between 300–950°C to prevent embrittlement

  • Excellent thermal fatigue strength

Stainless Steel Surface Finishing
Surface Finishes

Available in:
2B, No.4, HL, BA, pickled, polished, EPS

Alloy 255 vs 2205 vs 2507

Property 2205 255 2507
PREN
~34
≥40
42–45
Strength
High
Higher
Very high
Cost
$
$$
$$$
Acid Resistance
Good
Excellent
Excellent
Best For
General duplex
Seawater & chemical
Extreme chloride
Macro photograph showing the duplex microstructure of Alloy 255 stainless steel, with interlocking ferrite and austenite phases in contrasting colors.

Microstructure & Metallurgy

  • Balanced 50–50 ferrite–austenite duplex structure

  • High nitrogen stabilizes austenite & increases toughness

  • Ferrite phase improves SCC resistance

  • High Cr–Mo–N boosts pitting resistance

  • Controlled welding prevents formation of intermetallic phases

Industrial Applications

Marine & Offshore

  • Seawater piping

  • Firefighting systems

  • Heat exchangers

  • Riser tubes, splash-zone components

Desalination

  • Multi-stage flash (MSF) units

  • RO pumps and manifolds

  • Brine heaters

Chemical & Petrochemical

  • Reactors, tanks, scrubbers

  • Acid transfer piping

  • Evaporators

Pulp & Paper

  • Bleaching equipment

  • Black liquor processing

Oil & Gas

  • Downhole components

  • Sour service piping

  • Instruments & manifolds

Renewable Industry

  • Geothermal systems

  • Solar heater piping

  • Waste-to-energy plants

FAQs

Is Alloy 255 stronger than 316L and 2205?

Yes. Alloy 255 is 2× the strength of 316L and significantly stronger than 2205.

Can Alloy 255 be used in seawater?

Absolutely. It performs extremely well in hot, cold, flowing, and stagnant seawater.

Is Alloy 255 weldable?

Yes, but heat input must be controlled to avoid phase imbalance or intermetallic formation.

Is Alloy 255 magnetic?

Partially. Duplex alloys contain ferrite, making them lightly magnetic.

What is the temperature limit?

Recommended continuous service up to 300°C.

Why Kongfang Metal?

If you need Alloy 255 plates, pipes, fittings, bars, or custom-fabricated components, Kongfang Metal can supply complete solutions with mill certificates and global shipping.

📩 info@kongfangmetal.com

Kongfang Metal Factory
en_USEN
Send Your Inquiry Today

Scan to add on WeChat

Kongfang Metal WeChat-QR-Code