Alloy 926 (UNS N08926 / EN 1.4529) Stainless Steel Supplier

Available Forms

As a Alloy 926 stainless steel manufacturer in China, Kongfang Metal provide a wide range of Alloy 926 materials.

Cold Rolled Stainless Steel Sheet

Alloy 926 Sheet

Cold Rolled
Width: 1000 - 2000mm
Thickness: 0.3 - 6.0mm

Hot Rolled Stainless Steel Plate

Alloy 926 Plate

Hot Rolled
Width: 1000 - 2000mm
Thickness: 3 - 100mm

Cold-Rolled Stainless Steel Coil

Alloy 926 Cold-Rolled Coil

Cold Rolled
Width: 1000 - 2000mm
Thickness: 0.3 - 6.0mm

Hot-Rolled Stainless Steel Coil

Alloy 926 Hot-Rolled Coil

Hot Rolled
Width: 1000 - 2000mm
Thickness: 3 - 14mm

Stainless Steel Strip

Alloy 926 Strip

Width: 7 - 600mm
Thickness: 0.3 - 10mm

Stainless Steel Seamless Pipe

Alloy 926 Seamless Pipe

OD: ≤610mm
WT: 1 - 100 mm

Stainless Steel Welded Pipe

Alloy 926 Welded Pipe

OD: 6 - 3000mm
WT: 1 - 100 mm

Stainless Steel Round Bar

Alloy 926 Round Bar

Diameter: 1 - 200mm
Length: 100 - 12000mm

Stainless Steel Flat Bar

Alloy 926 Flat Bar

Width: 20 - 800 mm
Thickness: 3 - 60 mm

Stainless Steel Angle Bar

Alloy 926 Angle Bar

Side Length: 20 - 250 mm
Thickness: 3 - 35 mm

Stainless Steel Channel

Alloy 926 Channel

Height: 50 - 400 mm
Thickness: 4 - 20 mm

Stainless Steel H Beam

Alloy 926 H Beam

Height: 100 - 1000 mm
Thickness: 6 - 40 mm

If your system suffers from chloride corrosion, acid attack, or premature pitting failure, Alloy 926 is designed to solve that. It offers exceptional resistance to chlorides and acids, outperforming many stainless steels while remaining more cost-efficient than high-nickel alloys.

Comparison of Alloy 926 stainless steel with 316L and 904L showing superior resistance to chloride corrosion and pitting

Alloy 926 Equivalent Grades

ASTM / AISI UNS EN / W.Nr. DIN ISO GOST
Alloy 926
N08926
1.4529
X1NiCrMoCuN25-20-7
NiCr21Mo6CuN
03Х25Н20М2Т

Chemical Composition (Typical, wt.%)

C Cr Ni Mo Cu N Mn Si Fe
≤0.02
19–21
24–26
6.0–7.0
0.5–1.5
0.15–0.25
≤2.0
≤0.5
Balance

High Mo + N significantly boosts pitting and crevice corrosion resistance, while Ni stabilizes the austenitic structure under severe chloride stress.

Mechanical Properties (Room Temperature)

Property Metric Imperial
Tensile Strength
≥ 650 MPa
≥ 94 ksi
Yield Strength (0.2%)
≥ 295 MPa
≥ 43 ksi
Elongation
≥ 35%
≥ 35%
Hardness
≤ 230 HB
≤ 230 HB

You get excellent strength with high ductility, suitable for complex forming and pressure equipment.

Alloy 926 stainless steel demonstrating high PREN value and strong resistance to pitting, crevice corrosion, and chloride environments

Key Features

  • Exceptional resistance to pitting and crevice corrosion

  • Very high PREN value (≈42–45)

  • Excellent resistance to chloride stress corrosion cracking

  • Strong performance in sulfuric and phosphoric acids

  • Reliable in seawater and saline environments

  • Fully austenitic, non-magnetic structure

  • Easier fabrication than many nickel-based alloys

Alloy 926 is engineered for real-world chloride and acid exposure, not controlled lab conditions.

Performs well in:

  • Seawater and brackish water

  • Chloride-rich process streams

  • Sulfuric and phosphoric acid systems

  • Acidic condensates

  • Mixed chloride–acid environments

Compared to common grades:

  • Far superior to 316L in pitting and SCC resistance

  • Stronger than 904L under high chloride stress

  • Comparable corrosion resistance to 254SMO in many systems, often at lower total cost

If chloride-induced failure is your main concern, Alloy 926 is a proven upgrade.

Corrosion Resistance

Alloy 926 stainless steel performance in acid and chloride exposure compared with common stainless steel grades

Processing & Fabrication

Stainless Steel Machinability
Machining

More demanding than 316L; use rigid tooling and cooling.

Stainless Steel Formability
Forming

Good cold and hot formability.

Stainless Steel Weldability
Welding

TIG / MIG / SMAW using matching or Ni-based fillers

Stainless Steel Heat Treatment
Heat Treatment

No mandatory post-weld heat treatment in most cases.

Stainless Steel Surface Finishing
Surface Finish

Pickled, solution-annealed, or polished.

Industrial Applications

Alloy 926 is widely used where chlorides dominate the corrosion mechanism:

  • Seawater handling systems

  • Desalination and RO plants

  • Offshore and coastal piping

  • Heat exchangers and condensers

  • Chemical process piping

  • Oil & gas injection systems

  • Pressure vessels exposed to chlorides

When pitting, crevice corrosion, or SCC cannot be tolerated, Alloy 926 offers long-term reliability.

Alloy 926 vs 316L vs 904L vs 254SMO

Property316L904L254SMOAlloy 926
Cr (%)16–1819–2319–2119–21
Ni (%)10–1423–2817–1824–26
Mo (%)2–34–56–6.56–7
N (%)––0.18–0.220.15–0.25
PREN~25~35>42~42–45
Chloride ResistanceModerateVery goodExcellentExcellent
Typical UseGeneralChemicalSevere chlorideSevere chloride

FAQs

Is Alloy 926 better than 904L?

Yes. Alloy 926 offers much higher resistance to chlorides and pitting.

Is Alloy 926 similar to 254SMO?

In many environments, yes. Both provide excellent chloride resistance, with Alloy 926 offering higher Ni content.

What is the maximum service temperature?

Typically up to 300°C, depending on environment and stress.

Is Alloy 926 suitable for seawater?

Yes. It performs very well in static and flowing seawater systems.

Is Alloy 926 magnetic?

No. It is fully austenitic and non-magnetic.

Why Kongfang Metal?

  • Experience with high-alloy corrosion-resistant materials

  • Full product range and stable inventory

  • Support for international standards and documentation

  • Reliable global delivery

  • Technical assistance for material selection

If you’re unsure whether Alloy 926 or another grade fits your environment, share your chloride level, temperature, and pressure—we’ll help you choose correctly.

Kongfang Metal Factory
en_USEN
Send Your Inquiry Today

Scan to add on WeChat

Kongfang Metal WeChat-QR-Code