| ASTM (USA) | EN (Europe) | JIS (Japan) | GB (China) | GOST (Russia) | Description |
|---|---|---|---|---|---|
| 201 | 1.4372 | SUS 201 | 12Cr17Mn6Ni5N | 12Х15Г9НД | Austenitic, economical option with low nickel content. |
| 202 | 1.4373 | SUS 202 | 12Cr18Mn9Ni5N | 12Х17Г9АН4 | Similar to 201 but with higher manganese content. |
| 304 | 1.4301 | SUS 304 | 06Cr19Ni10 | 08X18H10 | Most common austenitic stainless steel, excellent corrosion resistance. |
| 304L | 1.4306 / 1.4307 | SUS 304L | 022Cr19Ni10 | 03X18H11 | Low-carbon version of 304, good for welding. |
| 316 | 1.4401 / 1.4436 | SUS 316 | 06Cr17Ni12Mo2 | 10Х17Н13М2 | Added molybdenum for increased resistance to pitting corrosion. |
| 316L | 1.4404 / 1.4435 | SUS 316L | 022Cr17Ni12Mo2 | 03X17H13M2 | Low-carbon version of 316, suitable for welding. |
| 317 | 1.4449 | SUS 317 | 06Cr19Ni13Mo3 | 07Х18Н15М3 | Similar to 316 but with higher molybdenum content for better corrosion resistance. |
| 310S | 1.4845 | SUS 310S | 06Cr25Ni20 | 20X23H18 | High-temperature resistance stainless steel. |
| 321 | 1.4541 | SUS 321 | 06Cr18Ni11Ti | 08X18H10T | Titanium-stabilized austenitic stainless steel for higher temperature use. |
| 347 | 1.4550 | SUS 347 | 06Cr18Ni11Nb | 08X18H12B | Niobium-stabilized for high-temperature stability. |
| 430 | 1.4016 | SUS 430 | 12Cr17 | 08X17 | Ferritic stainless steel with good formability and corrosion resistance. |
| 409 | 1.4512 | SUS 409 | 12Cr11Ti | 08X13 | Ferritic stainless steel used in automotive exhausts. |
| 410 | 1.4006 | SUS 410 | 12Cr13 | 12X13 | Martensitic stainless steel with good hardness and wear resistance. |
| 420 | 1.4021 / 1.4028 | SUS 420J1/J2 | 20Cr13 / 30Cr13 | 20X13 / 30X13 | High-carbon martensitic stainless steel, suitable for tools and blades. |
| 430F | 1.4104 | SUS 430F | 18Cr17 | 08X13F | Free-machining ferritic stainless steel, used in precision applications. |
| 440C | 1.4125 | SUS 440C | 9Cr18 | 95X18 | High-carbon martensitic stainless steel for high-wear applications like ball bearings. |
| 2205 (Duplex) | 1.4462 | SUS 329J3L | 022Cr23Ni5Mo3N | Duplex stainless steel with both high strength and corrosion resistance. | |
| 2507 (Super Duplex) | 1.4410 | – | 022Cr25Ni7Mo4N | Super duplex stainless steel for highly corrosive environments. | |
| 904L | 1.4539 | SUS 890L | 00Cr20Ni25Mo4.5Cu | 06ХН28МДТ | High-alloy austenitic stainless steel with extreme corrosion resistance. |
| 17-4PH | 1.4542 | SUS 630 | 0Cr17Ni4Cu4Nb | 04X17H13M2 | Precipitation-hardened stainless steel for high strength and toughness. |
| 303 | 1.4305 | SUS 303 | 06Cr19Ni10 | 12X18H10F | Free-machining austenitic stainless steel with added sulfur. |
| 309S | 1.4833 | SUS 309S | 06Cr23Ni13 | 20X23H13 | High-temperature resistant austenitic stainless steel. |
| 410S | 1.4000 | SUS 410S | 12Cr13 | 12X13 | Low carbon martensitic stainless steel for enhanced weldability. |
| 431 | 1.4057 | SUS 431 | 16Cr2Ni2 | 20Х17Н2 | Martensitic stainless steel with good corrosion resistance and toughness. |
| 440A | 1.4109 | SUS 440A | 8Cr17 | 65Х13 | Martensitic stainless with moderate corrosion resistance and high hardness. |
| 304H | 1.4948 | SUS 304H | 07Cr19Ni10 | 08X18H10 | High-carbon version of 304 for high-temperature applications. |
Explanation of Standards:
- ASTM: Commonly used in the United States and recognized globally, specifies properties and chemical composition.
- EN: European standard, widely adopted across Europe and internationally for industrial use.
- JIS: Japanese Industrial Standard, primarily used in Japan.
- GB: National standard of China.
- GOST: Russian state standards, applied within Russia and many former Soviet Union countries.