303 Stainless Steel Supplier
303 stainless steel (AISI 303 / UNS S30300) is a free-machining austenitic grade for turned, drilled and threaded parts.
Kongfang Metal supplies 303 stainless steel bar, cut blanks and machined products.

Added sulphur helps break chips during cutting, making it a practical choice for repeat production of fittings, fasteners, shafts and precision components.
Our stock, cutting and processing services help you prepare material for your next production run. Send your drawing or the size and quantity you need to get started.
Available Forms and Supply Options
Kongfang Metal supplies 303 round, hexagonal and square bar from stock and ordered production, with cutting and machining services for your finished parts. Round bar is our broadest stock range, followed by hexagonal bar. Square bar is supplied in regular sizes and to order.
Round bar
Hexagonal bar
Square bar
Round Bar
For CNC turning and automatic-lathe work, we supply hot-rolled, cold-drawn and bright round bar, together with larger forged sizes. Match the starting diameter, straightness and surface to your feeder, collet and machining allowance.
| Round bar form | Diameter mm | Typical length mm | Supply options |
|---|---|---|---|
| Hot rolled | Ø12–200 | 3,000–6,000; cut to length | Regular sizes stocked; large diameters and special lengths to order |
| Cold drawn or bright | Ø3–80 | 3,000–6,000; shorter cut lengths | Regular small and medium diameters stocked; precision requirements to order |
| Forged | Ø200–350 reference range | 1,000–4,000 | Made to order; annealing, peeling and rough-turning options |
Forged-bar dimensions follow the agreed forging and machining requirements.
Regularly stocked round-bar diameters:
- Hot rolled: 16, 20, 25, 30, 40, 50, 60, 80 and 100 mm.
- Cold drawn or bright: 6, 8, 10, 12, 16, 20, 25, 30, 40 and 50 mm.
Hexagonal and Square Bar
These sections suit fittings, nuts, spacers and parts that retain flats after machining. AF means width across flats for a hexagon; square-bar dimensions refer to the side length.
| Bar form | Available section mm | Typical length mm | Supply options |
|---|---|---|---|
| Hexagonal bar | AF 6–65 | 3,000–6,000; cut to length | Regular AF sizes stocked; special sizes and tolerances to order; larger sections can be machined |
| Square bar | 6 × 6 to 60 × 60 | 3,000–6,000; cut to length | Regular sizes from stock; non-standard and larger sections mainly to order, including hot-worked or milled options |
- Regular hexagonal stock sizes: AF 8, 10, 12, 14, 17, 19, 22, 24, 27, 30, 32, 36 and 41 mm.
- Regular square-bar stock sizes: side lengths of 10, 12, 16, 20, 25, 30 and 40 mm.
Send the size and quantity you need for current stock and delivery details.
Delivery Conditions and Processing
The manufacturing condition and surface finish serve different purposes. We can combine the agreed bar condition with the surface preparation and cutting needed for your job.
| Condition or process | Product options | Order details |
|---|---|---|
| Hot rolled | Medium and large round bar | Black surface; annealed condition and peeling or turning as ordered |
| Cold drawn | Round, hexagonal and square bar | Bright surface; diameter, AF or side tolerance, straightness and surface quality |
| Peeled or turned | Round bar | Finished diameter and machining allowance per side |
| Ground or polished | Precision round bar | Diameter tolerance, such as h9 or h11, and finish specified on the order |
| Cut to length | All bar forms | Length tolerance, end-face requirements, minimum cutting charge and ownership of offcuts |
Cut Blanks and Machined Parts
We manufacture and supply cut blanks and machined stainless steel components to drawing. Finished dimensions, threads, critical surfaces and inspection requirements guide the starting section and the material left for machining. Our material documentation links the mill test certificate (MTC) to the heat identification.
For an initial enquiry, a drawing or a description of the part is enough. We will help clarify the remaining material and supply details.
303 Stainless Steel Grades and Standards
303 is commonly identified as UNS S30300. EN 1.4305, named X8CrNiS18-9, is the related European free-machining grade. Specify the product standard alongside the grade so that the order and certificate describe the same material.
| Designation | How to use it when ordering |
|---|---|
| 303 / UNS S30300 | Use ASTM A582/A582M for free-machining stainless steel bars, with the required edition and delivery condition |
| EN 1.4305 / X8CrNiS18-9 | Use EN 10088-3 for the applicable long product and delivery condition |
| SUS303 | State the applicable JIS product standard and the requirements on your drawing |
| 303Se / UNS S30323 | A separate selenium-bearing grade; identify it explicitly if the drawing calls for it |
ASTM A582/A582M covers hot-finished and cold-finished free-machining bars, including rounds, squares and hexagons. ASTM A276/A276M covers bars other than free-machining types, so it is not an interchangeable specification for a 303 bar order.
Chemical Composition
The comparison below separates the published US 303 composition reference from the EN 1.4305 long-product limits. It is useful when checking whether a proposed alternative matches the chemistry required by the order.
| Element | 303 / UNS S30300 reference | EN 1.4305 long products |
|---|---|---|
| Carbon C | ≤0.15 | ≤0.10 |
| Silicon Si | ≤1.00 | ≤1.00 |
| Manganese Mn | ≤2.00 | ≤2.00 |
| Phosphorus P | ≤0.20 | ≤0.045 |
| Sulphur S | ≥0.15 | 0.15–0.35 |
| Chromium Cr | 17.0–19.0 | 17.0–19.0 |
| Nickel Ni | 8.0–10.0 | 8.0–10.0 |
| Nitrogen N | — | ≤0.11 |
| Copper Cu | — | ≤1.00 |
Values are percent by mass. A dash means no value is listed in the US reference used here. Acceptance limits follow the product standard and edition specified on the order.
When checking incoming 303 against a 304 alternative, look at the sulphur result as well as chromium and nickel on the MTC. Match the heat number on that certificate to the material identification.
Mechanical Properties by Product Form
Bar size and delivery condition affect strength and elongation. A bright bar and a solution-annealed hot-finished bar should therefore be compared using the requirements for their respective product forms.
EN 1.4305 Bright Bar at Room Temperature
| Section dimension t in mm | 0.2% proof strength minimum MPa | Tensile strength MPa | Elongation A minimum % |
|---|---|---|---|
| 5 ≤ t ≤ 10 | 400 | 600–950 | 15 |
| 10 < t ≤ 16 | 400 | 600–950 | 15 |
| 16 < t ≤ 40 | 190 | 500–850 | 20 |
| 40 < t ≤ 63 | 190 | 500–850 | 20 |
| 63 < t ≤ 160 | 190 | 500–750 | 35 |
EN 10088-3:2023 bright-bar reference values; t is diameter for rounds and width across flats for hexagons. The table starts at 5 mm because smaller dimensions have separate provisions, including agreed elongation requirements.
EN 1.4305 Solution-Annealed Long Products
| Product scope | 0.2% proof strength minimum MPa | Tensile strength MPa | Elongation A minimum % |
|---|---|---|---|
| Bars and sections up to 160 mm, excluding bright products | 190 | 500–750 | 35 |
EN 10088-3:2023 reference values. Separate provisions apply to bars and sections below 35 mm with final cold deformation and hot-formed bars and sections below 8 mm. For rod, only the tensile-strength requirement in this reference applies.
For an ASTM order, state the required bar condition and mechanical requirements under ASTM A582/A582M. Your material certificate should identify the supplied condition and the tests required by that order.
Machining 303 Stainless Steel
Sulphur forms manganese sulphide inclusions that help chips break and can improve tool life and the machined finish. This is why 303 is widely chosen for screw-machine work and repeated turning operations.
For production purchasing, compare the starting bar as well as the grade. Three details are especially useful:
- Bar feeding and gripping: match diameter tolerance, straightness and bar length to the machine and feeder.
- Material removal: allow enough stock for facing and finishing without buying an unnecessarily oversized section.
- The finished surface: identify threads, sealing faces, fits and surface roughness on the drawing, so these features receive the right inspection.
For a repeat order, retain the approved bar condition and surface requirements in the purchasing specification. When changing the material source or delivery condition, a trial on the actual part can establish the cutting settings and finish before the full run.
The useful cost comparison is the finished component: material yield, cutting time, tool changes, deburring and rejected parts all matter. A machinability rating alone does not predict a fixed reduction in cycle time.

Corrosion Resistance and Service Conditions
303 suits many machined components used in mild, relatively dry environments. Its sulphide inclusions reduce resistance to pitting and crevice corrosion compared with 304, especially where chlorides and retained moisture are present.
For a part exposed to salt spray, cleaning chemicals or liquid held in a recess, review the service environment before selecting 303. Consider drainage, temperature, cleaning and the finished surface. A component that machines easily still needs the right corrosion resistance in use.
Where corrosion resistance drives the decision, compare 304 stainless steel or 316L stainless steel against the actual exposure. For food-contact or hygienic equipment, include the contact conditions, cleaning process and applicable compliance requirements in material selection.
Welding Forming and Heat Treatment

Welding
303 is a poor choice for parts that need substantial welding because the sulphur added for machining restricts weldability. For a welded assembly, 304L or 316L is usually a more suitable starting point for material selection. If an existing design requires welding 303, use a qualified welding procedure to establish the joint requirements, consumable and acceptance tests.

Forming
303 has lower ductility than 304 and is better suited to machining than severe cold forming. For a component with deep drawing, heavy bending or cold heading, compare a more formable grade before committing the tooling and material.

Heat Treatment
303 is not hardened by conventional quenching and tempering. Cold working can increase strength, but it also changes ductility and machining behaviour. If the part needs high hardness or a defined heat-treated strength, compare a suitable hardenable grade, such as 17-4PH, with the design requirements.
For heated components, include the maximum metal temperature, exposure time and load in the material assessment. Oxidation resistance alone does not establish the allowable stress or service life of a loaded part.
303 Compared With Other Stainless Steels
| Material | A useful starting point when | What to compare next |
|---|---|---|
| 303 | Repeated turning, drilling and threading are major production operations | Bar condition, finished dimensions and service exposure |
| 304 or 304L | Forming or welding is central to the part | Fabrication sequence, surface finish and corrosion requirements |
| 316L | Corrosion resistance in a more demanding environment is important | Chlorides, temperature, crevices and cleaning conditions |
| 17-4PH | The design calls for higher strength from heat treatment | Required aging condition, mechanical properties and corrosion exposure |
For a closer comparison of machining, fabrication and service conditions, read 303 vs 304 stainless steel.
Applications for Machined Components
303 is used for fittings, fasteners, valve components, shafts, bushings and instrument parts. The buying requirement changes with the part:
- Threaded fittings and fasteners: identify the thread form, finished flats, burr control and any sealing surface.
- Shafts and bushings: show fits, concentricity, surface roughness and the portion of the bar that will be removed.
- Valve and instrument components: include the wetted medium, sealing requirements and cleaning conditions.
- Automatic-lathe parts: specify feeder-compatible bar lengths, straightness and the starting section tolerance.
These details help us supply material and processed products that fit the manufacturing job, rather than quote from the finished diameter alone.
Material Preparation and Delivery
Our warehousing and processing services connect the stock material, prepared blanks, documentation and packing. For cut material, we maintain identification through preparation and agree the marking needed on pieces or bundles. This helps your receiving team match material to the MTC before it enters production.
Protective wrapping and suitable packing help preserve prepared surfaces during handling and transport. Export orders can include the agreed packing, piece identification and shipping documentation in the delivery arrangements.


Request a 303 Quote
Send your drawing, product form, size, quantity and application. If some details are still being finalised, send what you have; we can clarify the material and supply requirements with you.
Example 303 Bar Enquiry
303 / UNS S30300 round bar to ASTM A582/A582M, 20 mm diameter × 3,000 mm length, 500 kg. Ground finish; diameter tolerance h9. MTC and heat identification required. Delivery to Rotterdam, Netherlands; required delivery date to be agreed.
For a Formal Quotation
Include as applicable:
- Grade, product standard and required edition.
- Diameter, width across flats or other section dimensions, tolerances and lengths.
- Delivery condition, surface finish and machining allowance.
- Quantity, destination and required delivery date.
- Drawing revision, critical features, inspection and material documentation.
- Packing and identification requirements.
Frequently Asked Questions
Is 303 stainless steel magnetic?
303 is generally non-magnetic in the annealed condition, but cold working can increase its magnetic response. A magnet test alone cannot identify the grade. If low magnetic permeability is a functional requirement, specify the limit and test method for the supplied product.
Does 303 stainless steel rust?
It can rust or stain under unsuitable exposure, especially with chlorides, trapped moisture or surface contamination. For a wet or corrosive application, compare the environment and cleaning conditions with a more corrosion-resistant grade.
Can 303 replace 304?
303 can be a useful alternative for a machined part when its corrosion resistance and mechanical properties meet the design. For parts requiring welding, severe forming or greater corrosion resistance, retain or compare 304 rather than changing the grade for machining convenience alone.
Is 303 the same as 1.4305?
EN 1.4305 is the related European free-machining grade. Its composition limits and product requirements are not identical to every US 303 specification. Use the grade and product standard on the drawing or order to check an alternative.
Can 303 be polished?
A machined 303 surface can be finished or polished. For a visible or sealing surface, specify the required roughness or agree a reference sample so that the finish can be inspected consistently.
Technical References
Technical data and product standards
ASTM A582/A582M — free-machining stainless steel bars
BSSA: US grade compositions; EN long-product compositions; bright-bar properties; other long-product properties; free-machining grades.